Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.MAGNUM ABS resins offer a wide range of processability and impact resistance for low gloss injection molding applications. Combined with heat resistance and tensile and flexural strength, MAGNUM ABS resins are used in a wide variety of injection molding applications.MAGNUM 348 ABS resin is a low gloss, low impact strength resin with good processability. MAGNUM 348 has a slight advantage in melt flow rate and impact strength over MAGNUM 341.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Elongation at Yield 2.3 %
2.3 %
ISO Data
Tensile Modulus 1.79 GPa
260 ksi
ASTM Data
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO Data, Low Temp
1.60 J/cm²
7.61 ft-lb/in²
ISO Data
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
Unannealed; ASTM Data
Vicat Softening Point 104 °C
219 °F
Flammability, UL94 HB