Material Notes:
Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent processability.Applications: Cosmetic packaging; containers for freezer; disposable packages with high transparency. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792A
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 1.05 GPa
152 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
10 N; ASTM D1525
Optical Properties Metric English Comments
Haze 18 %
18 %
ASTM D1003