Mechanical Properties Metric English Comments
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature -18.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
Compression Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de..
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.590 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Izod Impact, Notched 0.590 J/cm

@Temperature -40.0 °C
1.11 ft-lb/in

@Temperature -40.0 °F
50%RH; ASTM D256
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.590 J/cm

@Temperature -40.0 °C
1.11 ft-lb/in

@Temperature -40.0 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.590 J/cm

@Thickness 6.35 mm
1.11 ft-lb/in

@Thickness 0.250 in
ASTM D256
LG Chemical MI-770 MIPS
Izod Impact, Notched 0.590 J/cm

@Temperature -20.0 °C
1.11 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer
PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive..