Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -40.0 °C |
1.11 ft-lb/in @Temperature -40.0 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -40.0 °C |
1.11 ft-lb/in @Temperature -40.0 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 6.35 mm |
1.11 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical MI-770 MIPS |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -20.0 °C |
1.11 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive.. |