Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -20.0 °C |
1.31 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.3%); ASTM-D256 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.9%); ASTM-D256 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.4%); ASTM-D256 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -20.0 °C |
1.31 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4524WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resis.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.8%); ASTM-D256 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar CN005 Copolyester, High Flow Grade Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1218 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, high thermal resistanceInformation provided by Cossa Po.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0560 GFCTG Polypropylene, 30% Mixed Filler PP homopolymer 30% mixed fillerGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HI 0508 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber Characteristics: 17% glass fibre filled |
|||
Izod Impact, Notched | 0.700 - 1.10 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.31 - 2.06 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer CP 202XP is a high melt flow rate heterophasic copolymer designed to achieve parts with high stiffness and impact strength resistance, low warpage, and excellent surface appearance. Its applications.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 204 Injection Molding Polypropylene Description: CP 204 is a high melt flow rate heterophasic copolymer with general purpose additive package. This product exhibits excellent processing performance, with good stiffness and impact stre.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -20.0 °C |
1.31 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |