Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde.. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.3%); ASTM-D256 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.5%); ASTM-D256 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.4%); ASTM-D256 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -20.0 °C |
1.31 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4524WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resis.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASTIR HG 0808 Polystyrene High gloss polystyreneHigh impact resistance, good physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HI 0508 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber Characteristics: 17% glass fibre filled |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 401 HC Injection Molding Polypropylene Description: CP 401HC is a medium melt flow rate heterophasic copolymer, specially designed to achieve high stiffness/impact strength balance. This product offers good surface appearance and process.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer CP 202XP is a high melt flow rate heterophasic copolymer designed to achieve parts with high stiffness and impact strength resistance, low warpage, and excellent surface appearance. Its applications.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 204 Injection Molding Polypropylene Description: CP 204 is a high melt flow rate heterophasic copolymer with general purpose additive package. This product exhibits excellent processing performance, with good stiffness and impact stre.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -20.0 °C |
1.31 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |