Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 24.8 MPa @Strain 300 % |
3600 psi @Strain 300 % |
ASTM D412 |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,.. |
|||
Tensile Stress | 24.8 MPa @Strain 0.250 %, Temperature -20.0 °C |
3600 psi @Strain 0.250 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Tensile Stress | 24.8 MPa @Strain 6.00 %, Temperature 60.0 °C |
3600 psi @Strain 6.00 %, Temperature 140 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 24.8 MPa @Strain 17.9 %, Temperature 90.0 °C |
3600 psi @Strain 17.9 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |