Polymer Property : Tensile Stress = 3600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 24.8 MPa

@Strain 300 %
3600 psi

@Strain 300 %
ASTM D412
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane
Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,..
Tensile Stress 24.8 MPa

@Strain 0.250 %,
Temperature -20.0 °C
3600 psi

@Strain 0.250 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Tensile Stress 24.8 MPa

@Strain 6.00 %,
Temperature 60.0 °C
3600 psi

@Strain 6.00 %,
Temperature 140 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 24.8 MPa

@Strain 17.9 %,
Temperature 90.0 °C
3600 psi

@Strain 17.9 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers