Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790-95 |
Multibase Multi-Pro® 2510 XGW High Gloss Polypropylene PP High Gloss compound formulated for small appliances such as food-processors and coffee machines. This product is high heat stabilized for use in irons and other appliances with elevated temperat.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
PolyOne Lubri-Tech™ ATH-000/5M Acetal-Homopolymer
(discontinued **) Description/Features:Molybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)
(discontinued **) Description/Features:Mica FilledInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | Conditioned; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Strength | 34.5 MPa | 5000 psi | |
SGL Carbon Group EK 40 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Flexural Strength | 34.5 - 172 MPa | 5000 - 25000 psi | |
Du-Co Ceramics S-699 Alumina Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Aclo Accucomp Polypropylene CPO425BAV Automotive Approved Copolymer Expandable Grade |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided.. |
|||
Flexural Strength | 34.5 - 89.6 MPa | 5000 - 13000 psi | Compared to 500 for concrete |
Abatron AboJet Structural Crack-Injection Resin Structural crack injection resin for foundations, dikes, columns, load-bearing walls and structures. Offers strength, performance, durability, cost effectiveness and restoration instead of demoliti.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified Information provided by Asahi Thermofil |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Americas Styrenics STYRON® 487 High Impact Polystyrene Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Techmer ES Statiblend® PP TM10 BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightFeatures: ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.. |
|||
Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer Information provided by Chase Plastics. |