Aclo Accucomp Polypropylene CPO425BAV Automotive Approved Copolymer Expandable Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polypropylene CPO425BAV Automotive Approved Copolymer Expandable Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
MD; ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.20 GPa
174 ksi
ASTM D638
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
Flame Spread 25 mm/min
0.98 in/min
FMVSS