Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 38.0 MPa | 5510 psi | |
Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour sc.. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | Condition A; ASTM D790 |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PPC TS15020E Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | >= 38.0 MPa | >= 5510 psi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM 825EF High Impact Polystyrene Grade 825EF is a high impact polystyrene designed for extrusion and hot molding application. It is suited for hot molded deep drawn industrial packages and multilayer shaped sheet production via ex.. |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
BASF Capron® 8224 HSL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
Teknor Apex Sinpolene MFP 22KA2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ISO 178 |
Unitika EX-1020K PA6, Conditioned Conducting nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | GB/9341 |
Zhejiang Juner PP430R Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ISO 178 |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ISO 178 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EC6600 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Lithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Excellent printabilityMatte surface finishHigh hea.. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | cond; ISO 178 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Flexural Strength | 38.0 MPa | 5510 psi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PH-55Y Polystyrene - Food Medium impact |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339W10L1 Wollastonite Reinforced |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436G5M25CL Glass/Mineral Reinforced Coupled |
|||
Flexural Strength | 38.0 MPa | 5510 psi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Strength | 38.0 MPa @Thickness 19.0 mm |
5510 psi @Thickness 0.750 in |
ASTM D790 |
3A Composites Core Materials AIREX® PXw.420 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |
|||
Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 164 Polypropylene, Mineral Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
Polykemi AB POLYfill PPC T5020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 38.0 MPa @Temperature 23.0 °C |
5510 psi @Temperature 73.4 °F |
2mm/min; 80x10x4mm; ISO 178 |
SYNTHOS Krasten® 562E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo.. |