Unitika EX-1020K PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Unitika
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika EX-1020K PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conducting nylonInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Water Absorption 1.3 %

@Time 86400 sec
1.3 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.20 mm
0.010 in/in

@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.012 cm/cm

@Thickness 3.20 mm
0.012 in/in

@Thickness 0.126 in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ISO 2039
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-1/-2
Elongation at Break 38 %
38 %
ISO 527-1/-2
Tensile Modulus 1.20 GPa
174 ksi
ISO 527-1/-2
Flexural Strength 38.0 MPa
5510 psi
ISO 178
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179-1
Charpy Impact, Notched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179-1
Electrical Properties Metric English Comments
Volume Resistivity 10 ohm-cm
10 ohm-cm
IEC 60093