Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 1.0 - 2.5 g/10 min

@Load 0.325 kg,
Temperature 270 °C
1.0 - 2.5 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 1.50 GPa
218 ksi
Flexural Strength 38.0 MPa
5510 psi
Flexural Modulus 1.35 GPa
196 ksi
Charpy Impact Unnotched 1.80 J/cm²

@Temperature -20.0 °C
8.57 ft-lb/in²

@Temperature -4.00 °F
4.60 J/cm²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
Vicat Softening Point 116 °C
241 °F
B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C
1760 °F
at 3 mm
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F