Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Entec
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 10.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 16.0 %
16.0 %
ASTM D638
Elongation at Yield 6.00 %
6.00 %
ASTM D638
Flexural Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 2.069 GPa
300.1 ksi
tangent; ASTM D790
Izod Impact, Notched 0.290 J/cm

@Thickness 3.17 mm
0.543 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648