Mechanical Properties Metric English Comments
Flexural Strength 45.0 - 60.0 MPa
6530 - 8700 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Flexural Strength 45.0 - 60.0 MPa
6530 - 8700 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Flexural Strength 35.0 - 60.0 MPa
5080 - 8700 psi
Transverse
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite
MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev..
Flexural Strength 50.0 - 60.0 MPa
7250 - 8700 psi
ISO 178
Raschig Group EN 5004 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Flexural Strength 50.0 - 60.0 MPa
7250 - 8700 psi
ISO 178
Raschig Group EN 5007 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Flexural Strength 30.0 - 60.0 MPa
4350 - 8700 psi
ASTM D790
Raschig Group PiMC 1221 High gloss
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Strength 30.0 - 60.0 MPa
4350 - 8700 psi
ASTM D790
Raschig Group PiMC 1241 Sanitary, uni color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Strength 30.0 - 60.0 MPa
4350 - 8700 psi
ASTM D790
Raschig Group PiMC 1249 Sanitary, mix color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Strength 30.0 - 60.0 MPa
4350 - 8700 psi
ASTM D790
Raschig Group PiMC 1949 Granite colors