Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.28 - 3.00 GPa | 330 - 435 ksi | Average value: 2.63 GPa Grade Count:4 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Compressive Modulus | 2.70 - 3.00 GPa | 392 - 435 ksi | Average value: 2.84 GPa Grade Count:5 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |