Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 1020 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 7.06 GPa

@Strain 0.330 %,
Temperature 40.0 °C
1020 ksi

@Strain 0.330 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Secant Modulus 7.06 GPa

@Strain 0.330 %,
Temperature 40.0 °C
1020 ksi

@Strain 0.330 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Secant Modulus 7.00 GPa

@Strain 1.05 %,
Temperature -20.0 °C
1020 ksi

@Strain 1.05 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Secant Modulus 7.03 GPa

@Strain 2.30 %,
Temperature -20.0 °C
1020 ksi

@Strain 2.30 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Secant Modulus 7.00 GPa

@Strain 0.250 %,
Temperature 23.0 °C
1020 ksi

@Strain 0.250 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Secant Modulus 7.07 GPa

@Strain 1.50 %,
Temperature -40.0 °C
1020 ksi

@Strain 1.50 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..