Mechanical Properties Metric English Comments
Gardner Impact 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
ASTM D5420
Network Polymers Softflex® 2701
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Gardner Impact 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
ASTM D5420
Network Polymers Softflex® 2701T Transparent
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Gardner Impact 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
ASTM D3029
Flint Hills AP5325-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Nucleated and heat stabilizedApplications: Injection molding: large, thin wall automotive interior parts.Former Huntsman polypropyle..
Gardner Impact 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
ASTM D3029
Flint Hills AP6112-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma..
Gardner Impact 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
ASTM D3029
Flint Hills AP6120-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma..
Gardner Impact 27.0 J

@Temperature 23.0 °C
19.9 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills P5M6K-080 Polypropylene Random Copolymer
Features: Clarified, Gamma Radiation Sterilizable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: Disposable Syringes. This product is not rec..
Gardner Impact 27.0 J
19.9 ft-lb
ASTM D3029
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant
Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processabilityApplications: furniture, small..
Gardner Impact 27.0 J
19.9 ft-lb
ASTM D3029
SABIC Innovative Plastics NORYL SPN420 PPE+PS
Superior Productivity plus heat and impact resistance. Excellent processability.
Gardner Impact 27.0 J
19.9 ft-lb
ASTM D3029
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific)
Superior Productivity plus heat and impact resistance. Excellent processability.
Gardner Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
ASTM D3029
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific)
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.
Gardner Impact >= 27.0 J
>= 19.9 ft-lb
Spartech DKE® 450 450 PVC/Acrylic Fire Rated Sheet  (discontinued **)
Data provided by the manufacturer.
Gardner Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
ASTM D3029
SABIC Innovative Plastics PREVEX W20 PPE+PS
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.