Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 2701 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 2701T Transparent Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
Flint Hills AP5325-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Nucleated and heat stabilizedApplications: Injection molding: large, thin wall automotive interior parts.Former Huntsman polypropyle.. |
|||
Gardner Impact | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
Flint Hills AP6112-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Gardner Impact | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
Flint Hills AP6120-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Gardner Impact | 27.0 J @Temperature 23.0 °C |
19.9 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Flint Hills P5M6K-080 Polypropylene Random Copolymer Features: Clarified, Gamma Radiation Sterilizable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: Disposable Syringes. This product is not rec.. |
|||
Gardner Impact | 27.0 J | 19.9 ft-lb | ASTM D3029 |
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processabilityApplications: furniture, small.. |
|||
Gardner Impact | 27.0 J | 19.9 ft-lb | ASTM D3029 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Gardner Impact | 27.0 J | 19.9 ft-lb | ASTM D3029 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific) Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Gardner Impact | 27.0 J @Temperature -40.0 °C |
19.9 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Gardner Impact | >= 27.0 J | >= 19.9 ft-lb | |
Spartech DKE® 450 450 PVC/Acrylic Fire Rated Sheet
(discontinued **) Data provided by the manufacturer. |
|||
Gardner Impact | 27.0 J @Temperature -40.0 °C |
19.9 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
SABIC Innovative Plastics PREVEX W20 PPE+PS Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |