Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 110 - 160 MPa | 16000 - 23200 psi | ISO.2039-2 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Ball Indentation Hardness | 110 - 160 MPa | 16000 - 23200 psi | ISO.2039-2 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Ball Indentation Hardness | 50.0 - 160 MPa | 7250 - 23200 psi | Average value: 138 MPa Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Ball Indentation Hardness | 80.0 - 160 MPa | 11600 - 23200 psi | Average value: 114 MPa Grade Count:10 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Ball Indentation Hardness | 50.0 - 160 MPa | 7250 - 23200 psi | Average value: 132 MPa Grade Count:5 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |