Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 80.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 80.0 MPa
11600 psi
ISO2039.1 DIN.53456
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH
Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom..
Ball Indentation Hardness 80.0 MPa
11600 psi
ISO2039.1 DIN.53456
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH
Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T..
Ball Indentation Hardness 80.0 - 270 MPa
11600 - 39200 psi
Average value: 180 MPa Grade Count:22
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Ball Indentation Hardness 80.0 - 160 MPa
11600 - 23200 psi
Average value: 114 MPa Grade Count:10
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Ball Indentation Hardness 80.0 MPa
11600 psi
ISO 2039
GEHR Plastics PVDF Polyvinylidene Fluoride
Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan..
Ball Indentation Hardness 80.0 MPa
11600 psi
ISO 2039-1
Styrolution Luran® S 767KE ASA
Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos..
Ball Indentation Hardness 80.0 MPa

@Load 36.5 kg,
Time 30.0 sec
11600 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Ball Indentation Hardness 80.0 MPa
11600 psi
ISO 2039-1
Styrolution Terluran® HI-12 ABS
Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® 1S XE 4224 nat PA1010
Product Description: Grilamid XE 4224 natural is a heat and UV stabilized high viscosity polyamide 1010 (PA1010), designed for extrusion. In addition the product can be used for thicker injection mo..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BG-15 PA6-GF15
Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BG-15 S PA6-GF15
Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BG-15/2 PA6-GF15
Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BG-30 EC PA6-GF30
Information provided by EMS Grivory
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BT 40 Z PA6
Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® LM-05 HX nat PA12
Product description: Grilamid LM-05 HX natural is a medium viscosity, heat-stabilized nanocomposite PA12 extrusion and injection molding grade. The special features of Grilamid LM-05 HX natural are:..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSGK-30/4 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X/4 is a heat stabilized PA 66 + PA 6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30/4 X has the foll..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSS/2 FA PA666
Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow ..
Ball Indentation Hardness 80.0 MPa

@Time 30.0 sec
11600 psi

@Time 0.00833 hour
DIN 53 456
Hippe PP Polypropylene
Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-..
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I
Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper..
Ball Indentation Hardness 80.0 MPa
11600 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-763 ABS - Flame Retardant
F.R. High Heat Weather Resistant
Ball Indentation Hardness 80.0 MPa

@Load 36.5 kg,
Time 30.0 sec
11600 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2650 Z4 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Ball Indentation Hardness 80.0 MPa
11600 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-763A ABS - Flame Retardant
F.R. High Heat
Ball Indentation Hardness 80.0 - 120 MPa
11600 - 17400 psi
Average value: 99.3 MPa Grade Count:26
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Ball Indentation Hardness 80.0 MPa
11600 psi
Fm=358N; Ø 50x4mm; ISO 2039-1
SYNTHOS Krasten® 336M High Impact Polystyrene
Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos.