Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 270 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 270 MPa
39200 psi
ISO 2039-1
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced
Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 270 - 360 MPa
39200 - 52200 psi
Average value: 320 MPa Grade Count:11
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50
Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-3H LF PA*-GF30
Grivory TH2V-3H LF is a glass fiber reinforced (30%), PTFE modified engineering thermoplastic based on semi-crystalline partially aromatic copolyamide. Polymer designation acc. ISO: PA6T/66 Polymer ..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: ..
Ball Indentation Hardness 270 MPa
39200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30
Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Ball Indentation Hardness 270 MPa
39200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HTV-3H1 nat PA6T/6I-GF30
Product description: Grivory HTV-3H1 natural is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-50 FA PA666-GF50
Information provided by EMS Grivory
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-50 PA666-GF50
Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50
Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-50 H PA6-GF50
Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-50 S PA6-GF50
Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin..
Ball Indentation Hardness 270 MPa
39200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50
Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac..
Ball Indentation Hardness 270 MPa
39200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Ball Indentation Hardness 270 MPa
39200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Ball Indentation Hardness 270 MPa
39200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45
Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation..
Ball Indentation Hardness 270 MPa

@Load 36.5 kg
39200 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Ball Indentation Hardness 270 MPa
39200 psi
HB 961/30; ISO 2039-1
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Ball Indentation Hardness 270 MPa
39200 psi
H 961/30; ISO 2039-1
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Ball Indentation Hardness 270 MPa
39200 psi
H 961/30; ISO 2039-1
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Ball Indentation Hardness 270 MPa
39200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30
Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl..
Ball Indentation Hardness 270 - 290 MPa
39200 - 42100 psi
Average value: 283 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Copyright © lookpolymers.com All Rights Reserved