Polymer Property : Ball Indentation Hardness = 310 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 310 MPa
45000 psi
ISO 2039-1
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data)
This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45
Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST..
Ball Indentation Hardness 310 MPa
45000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45
Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40
Product description: Grivory HTV-4H1 black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40
Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50
Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following ..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50
Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following ..
Ball Indentation Hardness 310 MPa
45000 psi
DAM; H 961/30; ISO 2039-1
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60
Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40
Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Ball Indentation Hardness 310 MPa
45000 psi
H 961/30; ISO 2039-1
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40
Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Ball Indentation Hardness 310 MPa
45000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-4 HY black 9205 PA6T/6I-GF40
Product description: Grivory HT1V-4 HY black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-4 HY bl..
Ball Indentation Hardness 310 - 330 MPa
45000 - 47900 psi
Average value: 322 MPa Grade Count:5
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..