Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 8990 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 62.0 MPa
8990 psi
DIN 53456
Ineos Nova S-4600 High Impact Compact Polystyrene  (discontinued **)
High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection mold..
Ball Indentation Hardness 62.0 - 106 MPa
8990 - 15400 psi
Average value: 85.5 MPa Grade Count:15
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Ball Indentation Hardness 62.0 - 105 MPa
8990 - 15200 psi
Average value: 92.5 MPa Grade Count:4
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Ball Indentation Hardness 62.0 - 68.0 MPa
8990 - 9860 psi
DIN 53 456
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer
Fluoropolymer material specifications.Information provided by Isoflon.
Ball Indentation Hardness 62.0 MPa

@Load 36.5 kg,
Time 30.0 sec
8990 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned)
Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent ..
Ball Indentation Hardness 62.0 MPa
8990 psi
358 N/30s; ISO 2039
Borealis ME266U Polypropylene Compound, Mineral Filled
ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. ..
Ball Indentation Hardness 62.0 MPa
8990 psi
H 385/30; ISO 2039
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer
Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well ..
Ball Indentation Hardness 62.0 MPa
8990 psi
H 385/30; ISO 2039
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h..
Ball Indentation Hardness 62.0 MPa
8990 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant
This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr..
Ball Indentation Hardness 62.0 - 99.0 MPa
8990 - 14400 psi
Average value: 85.3 MPa Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..