Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Borealis
Trade Name Xmod™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 has been designed for pillar trims, door panels and pockets, and central consoles.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
57 g/10 min

@Load 5.00 kg,
Temperature 230 °C
57 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 62.0 MPa
8990 psi
H 385/30; ISO 2039
Tensile Strength, Yield 26.0 MPa
3770 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 7.0 %
7.0 %
At 50 mm/min; ISO 527-2
Tensile Modulus 1.60 GPa
232 ksi
At 1 mm/min; ISO 527-2
Flexural Modulus 1.55 GPa
225 ksi
At 5 mm/min; ISO 178
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -20.0 °C
24.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
0.360 J/cm²

@Temperature -20.0 °C
1.71 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ISO 75-2
Vicat Softening Point 70.0 °C
158 °F
B (50N); ISO 306
150 °C
302 °F
A (10N); ISO 306
Shrinkage 1.5 %
1.5 %
Borealis Method
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Polymer Mass Temp
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F