Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 E Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 243R PC (Europe-Africa-Middle East) LEXAN 243R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD923A PC (Europe-Africa-Middle East) LEXAN FXD923A is a transparent/translucent, medium viscosity, flame retardent grade for light diffusion special effects. UV-stabilized. Color package may affect performance. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 143 PC (Europe-Africa-Middle East) LEXAN 143 is a medium viscosity U.V. stabilized multi purpose grade. LEXAN 143 is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 HH-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.50 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1/CF/20 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179 |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 216 NATURAL FA PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179-1 |
Unitika A1025GO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | double V-notch, rk=1.5 mm; DIN 53753 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | double V-notch, rk=1.5 mm; DIN 53753 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSG-50/4 PA666-GF50 Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 30.0 °C |
6.66 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 30.0 °C |
6.66 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | |
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 30.0 °C |
6.66 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |