Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP1364E2 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP1364E2 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer products.Availability: Africa & Middle East and Europe Uses: CapsClosuresCompoundingConsumer ApplicationsCupsFurnitureProcessing Method: Injection Molding and CompoundingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2/50
Elongation at Yield 8.0 %
8.0 %
ISO 527-2/50
Tensile Modulus 1.45 GPa
210 ksi
ISO527-2
Flexural Modulus 1.35 GPa
196 ksi
ISO 178
Izod Impact, Notched (ISO) 1.99 kJ/m²
0.950 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.294 J/cm²
1.40 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 320 °C
608 °F
ISO 3146
Crystallization Temperature 237 °C
459 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ISO 75-2/A
Vicat Softening Point 153 °C
307 °F
ISO 306/A50