Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.360 J/cm²

@Temperature 23.0 °C
1.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179
PolyOne Bergamid™ A70 G5 T Polyamide 66 (Nylon 66)
Information provided by PolyOne
Charpy Impact, Notched 0.360 J/cm²

@Temperature -30.0 °C
1.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)  (Unverified Data**)
Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f..
Charpy Impact, Notched 0.360 - 1.20 J/cm²
1.71 - 5.71 ft-lb/in²
Average value: 0.866 J/cm² Grade Count:10
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Charpy Impact, Notched 0.360 - 4.00 J/cm²
1.71 - 19.0 ft-lb/in²
Average value: 1.37 J/cm² Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Charpy Impact, Notched 0.360 J/cm²

@Temperature 23.0 °C
1.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Fibrolon® P 8540 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C..
Charpy Impact, Notched 0.360 J/cm²

@Temperature 23.0 °C
1.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Terralene® WF 6534 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber
Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla..
Charpy Impact, Notched 0.360 J/cm²

@Temperature -20.0 °C
1.71 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h..
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® C7640 Polybutylene Terephthalate (PBT), Super low warpage, Mineral filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.360 J/cm²

@Temperature -30.0 °C
1.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned)
Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and ..
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
1eA; ISO 179
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM
10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov..
Charpy Impact, Notched 0.360 J/cm²

@Temperature -30.0 °C
1.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Appryl® CZN 0525 Polypropylene, 25% Talc Filled
Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for interior trim applications, that required an excellent impact test associated with a high modul..
Charpy Impact, Notched 0.360 J/cm²

@Temperature -30.0 °C
1.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer
PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I..
Charpy Impact, Notched 0.360 J/cm²

@Temperature -30.0 °C
1.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Appryl® CZU 0525 Polypropylene, 25% Talc Filled
Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for exterior trim automotive applications, that required an excellent impact test associated with a..
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179
Vyncolit X611 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in..
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® GM-20 Acetal Co-polymer (POM), Low warpage, GF 20% reinforced
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..