Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vyncolit X611 Novolac Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit X611 Novolac Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. insulators, spacers, edge connectors, coil former, timer parts and computer componentsInformation provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
Powder Density; ISO 60
Density 1.65 g/cc
0.0596 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ISO 527
Elongation at Break 0.70 %
0.70 %
Tensile; ISO 527
1.5 %
1.5 %
Flexure; ISO 178
Tensile Modulus 15.0 GPa
2180 ksi
ISO 527
Flexural Strength 200 MPa
29000 psi
At Rupture; ISO 178
Flexural Modulus 14.5 GPa
2100 ksi
ISO 178
Compressive Strength 250 MPa
36300 psi
ISO 604
Charpy Impact Unnotched 0.950 J/cm²
4.52 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75 Af
Flammability, UL94 V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Shrinkage 0.15 %
0.15 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 93
Insulation Resistance 7.50e+10 ohm
7.50e+10 ohm
Wet; 24 hours in water; IEC 167
1.00e+11 ohm
1.00e+11 ohm
Dry; IEC 167
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243
Comparative Tracking Index 125 V
125 V
IEC 112
Descriptive Properties Value Comments
Color Black, Green
ISO type PF 2 C1
Main Filler Glass Fiber
Molding Method Compression, transfer, injection
Users viewing this material also viewed the following: