Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Arkema
Trade Name Appryl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 7.0 %
7.0 %
50 mm/min
Tensile Modulus 1.18 GPa
171 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
0.360 J/cm²

@Temperature -30.0 °C
1.71 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
10°C/min
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
Vicat Softening Point 71.0 °C
160 °F
50°C/hr; 50N