Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.310 - 1.30 J/cm²

@Temperature -30.0 - 30.0 °C
1.48 - 6.19 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.05 J/cm² Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Charpy Impact, Notched 0.310 - 0.370 J/cm²

@Temperature -30.0 - -30.0 °C
1.48 - 1.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.340 J/cm² Grade Count:2
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Charpy Impact, Notched 0.310 J/cm²

@Temperature -30.0 °C
1.48 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastapak 9921W PET  (discontinued **)
Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Charpy Impact, Notched 0.310 J/cm²

@Temperature -30.0 °C
1.48 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar GN101 PETG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.310 J/cm²
1.48 ft-lb/in²
ASTM D256
Plenco 1581 Polyester, Pellet, Injection Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Charpy Impact, Notched 0.310 J/cm²
1.48 ft-lb/in²
ASTM D256
Plenco 7556 Phenolic, Briquette, Transfer Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..
Charpy Impact, Notched 0.310 J/cm²

@Temperature -40.0 °C
1.48 ft-lb/in²

@Temperature -40.0 °F
Method B; Brittle Failure
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6
30% crystallinity. Information supplied by Elastomer Engineering.
Charpy Impact, Notched 0.310 J/cm²
1.48 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 601SA Polybutylene Terephthalate (PBT), Low density, Low wear, Mineral filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.310 J/cm²
1.48 ft-lb/in²
ASTM D256
Plenco 7552 Phenolic, Nodular, Injection Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..
Charpy Impact, Notched 0.310 J/cm²
1.48 ft-lb/in²
ASTM D256
Plenco 7591 Phenolic, Pellet, Transfer Molded
PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.