Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.700 - 3.20 J/cm²
3.33 - 15.2 ft-lb/in²
Average value: 1.23 J/cm² Grade Count:19
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Charpy Impact, Notched 0.600 - 3.20 J/cm²
2.86 - 15.2 ft-lb/in²
Average value: 1.58 J/cm² Grade Count:39
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Charpy Impact, Notched 0.300 - 3.20 J/cm²
1.43 - 15.2 ft-lb/in²
Average value: 0.979 J/cm² Grade Count:21
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Charpy Impact, Notched 1.60 - 3.20 J/cm²
7.61 - 15.2 ft-lb/in²
Average value: 2.22 J/cm² Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
Charpy Impact, Notched 1.60 - 3.20 J/cm²

@Temperature -30.0 - -30.0 °C
7.61 - 15.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.22 J/cm² Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
Charpy Impact, Notched 0.380 - 3.20 J/cm²
1.81 - 15.2 ft-lb/in²
Average value: 1.43 J/cm² Grade Count:9
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..