Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.412 - 0.539 J/cm | 0.772 - 1.01 ft-lb/in | Average value: 0.461 J/cm Grade Count:6 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Izod Impact, Notched | 0.210 - 0.540 J/cm | 0.393 - 1.01 ft-lb/in | Average value: 0.375 J/cm Grade Count:3 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Izod Impact, Notched | 0.440 - 0.540 J/cm @Thickness 6.35 mm |
0.824 - 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT1200M General Purpose PBT Information provided by Dowell Trading Company Ltd. |