Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2020 LO-GC Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2210 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E7364 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4218 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re.. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 4.00 mm |
18.7 ft-lb/in @Thickness 0.157 in |
ASTM D256 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 4.00 mm |
18.7 ft-lb/in @Thickness 0.157 in |
ASTM D256 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched | 10.0 J/cm @Temperature 23.0 °C |
18.7 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA860 Nylon 6.6, Impact Modified Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
2 m/s, Partial Break; ASTM D6110 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
2 m/s, Partial Break; ASTM D6110 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |