Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Engineered Plastics EPPC 2214C Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Engineered Plastics Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Plastics EPPC 2214C Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clear injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 22 g/10 min
22 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Notched 7.50 J/cm
14.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Unannealed; ASTM D648
150 °C
302 °F
Annealed; ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear, but thickness unknown