Polymer Property : Izod Impact, Notched = 2.70 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.39 - 1.44 J/cm

@Temperature -30.0 - -30.0 °C
2.60 - 2.70 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 1.43 J/cm Grade Count:4
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Izod Impact, Notched 0.320 - 1.44 J/cm
0.599 - 2.70 ft-lb/in
Average value: 0.597 J/cm Grade Count:37
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched 1.17 - 1.44 J/cm

@Thickness 6.35 mm
2.19 - 2.70 ft-lb/in

@Thickness 0.250 in
ASTM D256
PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber  (discontinued **)
Data provided by PolyOne.