Mechanical Properties Metric English Comments
Izod Impact, Notched 2.88 J/cm
5.40 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 2645 ABS, Impact Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 2.88 J/cm
5.40 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 545 ABS, General Purpose
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 2.88 J/cm
5.40 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1390 PPE+PS
Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL.
Izod Impact, Notched 2.88 J/cm
5.40 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1390 PPE+PS (Asia Pacific)
Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL.
Izod Impact, Notched 2.88 J/cm

@Thickness 3.17 mm
5.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 2.88 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
5.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 2.88 J/cm

@Temperature 23.0 °C
5.40 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton PV00A PA 6
LNP VERTON* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.88 J/cm

@Temperature 23.0 °C
5.40 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton PV00A PA 6 (Asia Pacific)
LNP* Verton* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.