PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.1 MPa
6400 psi
ASTM D638
Flexural Yield Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
ASTM D790
Izod Impact, Notched 2.88 J/cm

@Thickness 3.17 mm
5.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
0.5 inch; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
ASTM D249