Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.88 J/cm | 5.40 ft-lb/in | ASTM Data |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.88 J/cm | 5.40 ft-lb/in | ASTM Data |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.88 J/cm | 5.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1390 PPE+PS Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL. |
|||
Izod Impact, Notched | 2.88 J/cm | 5.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1390 PPE+PS (Asia Pacific) Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL. |
|||
Izod Impact, Notched | 2.88 J/cm @Thickness 3.17 mm |
5.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 2.88 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.40 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3003MC Black 1722 Description: BlackInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.88 J/cm @Temperature 23.0 °C |
5.40 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 LNP VERTON* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.88 J/cm @Temperature 23.0 °C |
5.40 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 (Asia Pacific) LNP* Verton* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |