Material Notes:
resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Yield Strength 16.0 MPa
2320 psi
ASTM D790
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Izod Impact, Notched 6.50 J/cm
12.2 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ASTM D789
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 200 °C
392 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F