Polymer Property : Charpy Impact Unnotched = 0.700 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Charpy Impact Unnotched 0.700 - 0.900 J/cm²
3.33 - 4.28 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Charpy Impact Unnotched 0.700 - 0.900 J/cm²
3.33 - 4.28 ft-lb/in²
Injection and Compression; ISO 179/1eU
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
Charpy Impact Unnotched 0.700 - 0.900 J/cm²
3.33 - 4.28 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Charpy Impact Unnotched 0.700 - 1.10 J/cm²
3.33 - 5.23 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Charpy Impact Unnotched 0.700 - 1.20 J/cm²

@Temperature 23.0 °C
3.33 - 5.71 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
Charpy Impact Unnotched 0.700 - 1000 J/cm²
3.33 - 4760 ft-lb/in²
Average value: 2.38 J/cm² Grade Count:25
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Lustran® QE 1455, Injection Grade  (discontinued **)
Injection molding grade, increased heat resistance, medium gloss.Applications: Automotive: interior parts.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renam..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Lustran® QE 1455/L2, Injection Grade  (discontinued **)
Injection molding grade, increased heat resistance, medium gloss, UV-stabilized grade.Applications: Automotive: body parts.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength  (d
Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed  (disc
Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic..
Charpy Impact Unnotched 0.700 - 3.00 J/cm²
3.33 - 14.3 ft-lb/in²
Average value: 1.97 J/cm² Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Charpy Impact Unnotched 0.700 - 2.90 J/cm²

@Temperature -40.0 - -20.0 °C
3.33 - 13.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.04 J/cm² Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Charpy Impact Unnotched 0.700 J/cm²
3.33 ft-lb/in²
LATI Latigray 52/11-01 CX/70 PP Homopolymer
Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value..
Charpy Impact Unnotched 0.700 - 0.900 J/cm²
3.33 - 4.28 ft-lb/in²
ISO 179
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group
Charpy Impact Unnotched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Vyncolit 4523 XB Novolac Phenolic
Organic and inorganic filled phenolic molding compound with good mechanical and thermal properties. Improved heat resistance compared to organic filled compounds.USES: Fuse holders, brush holders, ..
Charpy Impact Unnotched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Vyncolit X620/1 Novolac Phenolic
Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
Total PPC 4624WZ Polypropylene, Impact Copolymer
ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Covestro Apec® HT KU 1-9361 High-Heat Polycarbonate
Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated ..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Covestro Apec® HT KU 1-9363 High-Heat Polycarbonate, UV-Stabilized
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Charpy Impact Unnotched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Chi Mei Polyrex® PG-22 Polystyrene
TPE compound
Charpy Impact Unnotched >= 0.700 J/cm²
>= 3.33 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.Information ..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²
3.33 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Charpy Impact Unnotched 0.700 J/cm²
3.33 ft-lb/in²
LATI Laticonther 75 GR/50 PBT, 50% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
Charpy Impact Unnotched 0.700 J/cm² - NB
3.33 ft-lb/in² - NB
Average value: 4.68 J/cm² Grade Count:87
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..