Polymer Property : Charpy Impact Unnotched = 18.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.00 - 18.0 J/cm²

@Temperature -30.0 - -30.0 °C
23.8 - 85.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 10.5 J/cm² Grade Count:22
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Charpy Impact Unnotched 5.10 - 18.0 J/cm²
24.3 - 85.7 ft-lb/in²
Average value: 11.7 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..