Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 5.10 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -40.0 °C
24.3 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 GV50 Nylon 6 for injection molding, 50% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -40.0 °C
24.3 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 H-GV50 Nylon 6 for injection molding, 50% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 HH-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 5.10 - 18.0 J/cm²
24.3 - 85.7 ft-lb/in²
Average value: 11.7 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Charpy Impact Unnotched 5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eU
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179-1
Unitika A1025NO PA6, Flame Retardant, Conditioned
Information provided by Unitika Ltd.
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -20.0 °C
24.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h..
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179
Chi Mei Polylac® PA-758R ABS - Transparent
Transparent, Chemical Resistant
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -30.0 °C
24.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -30.0 °C
24.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179
BASF Ultradur B 4300 G4 High Speed Unc. 20% Glass Filled PBT
Ultradur B 4300 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap..
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179
BASF Nypel® 6030G HS DB BK 5830 30% Glass Filled PA6 (Dry)
Description: Nypel® 6030G HS DB BK5830 is a 30% glass fiber reinforced, heat stabilized, black pigmented, injection molding compound based on recycled PA6..Application: Nypel® 6030G HS DB BK5830..
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -30.0 °C
24.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa..
Charpy Impact Unnotched 5.10 J/cm²

@Temperature -20.0 °C
24.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSX65T20 is a 20% mineral filled grade intended for injection molding. Daplen KSX65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSX65T20 offe..