Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 22.0 J/cm² - NB @Temperature -40.0 - -30.0 °C |
105 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
Average value: 30.7 J/cm² Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | |
Ineos ABS Lustran® H801 High heat resistance, PC modified, low emission, increased flow.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | 47 HRC |
International Mold Steel DHA-World Die Cast & Forging Steel DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel |
|||
Charpy Impact Unnotched | 22.0 J/cm² @Temperature -30.0 °C |
105 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1505 Z 000000 PBT PBT, non-reinforced, injection molding, extrusion, impact modified |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering .. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179 |
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² - NB | 105 ft-lb/in² - NB | Average value: 28.4 J/cm² Grade Count:133 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an.. |
|||
Charpy Impact Unnotched | 22.0 J/cm² | 105 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTRODAL W Polyoxymethylene POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe.. |