Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTRODAL W Polyoxymethylene

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTRODAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTRODAL W Polyoxymethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe application within the vicinity of drinking water. The excellent machinability, dimensional stability and chemical resistance of the basic polyoxymethylene polymer remain. It confirms to food regulatory standards in accordance with BfR/FDA. POM W-plastics often serve as construction elements for bottling drinking water machinery.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Moisture Absorption 0.200 %

@Temperature 23.0 °C
0.200 %

@Temperature 73.4 °F
normal humidity; ISO 62
Water Absorption at Saturation 0.80 %

@Temperature 23.0 °C
0.80 %

@Temperature 73.4 °F
ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 84
84
test piece 10mm thick; ISO 2039-2
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Tensile Strength 63.0 MPa
9140 psi
5 mm/min; ISO 527-2
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ISO 527-2
Elongation at Break 31 %
31 %
ISO 527-2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-2
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 23.0 - 60.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 165 °C
329 °F
DSC, 10 K/m; ISO 3146
Maximum Service Temperature, Air 105 °C
221 °F
continuous
140 °C
284 °F
short term
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ISO 75-2
Vicat Softening Point 150 °C
302 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB

@Thickness 3.00 - 6.00 mm
HB

@Thickness 0.118 - 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 100 Hz
3.8

@Frequency 100 Hz
IEC 60250
3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0030

@Frequency 100 Hz
0.0030

@Frequency 100 Hz
IEC 60250
0.0080

@Frequency 1.00e+6 Hz
0.0080

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Color Natural
Food Compliance BfR: Yes
Food Compliance FDA Yes