Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.800 - 30.0 J/cm² | 3.81 - 143 ft-lb/in² | Average value: 6.23 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |