Polymer Property : Charpy Impact Unnotched = 39.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® 144 PC
UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco..
Charpy Impact Unnotched 8.20 J/cm²
39.0 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
Charpy Impact Unnotched 8.20 J/cm²
39.0 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
Charpy Impact Unnotched 8.20 J/cm²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179; DIN 53453
Zell-Metall Engineering Plastics Zellamid 1400 (PET)
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
Charpy Impact Unnotched 8.20 J/cm²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179; DIN 53453
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
Charpy Impact Unnotched 8.20 J/cm²
39.0 ft-lb/in²
ISO 179-1
Unitika A1030TF PA6, Dry
Lubricating nylonInformation provided by Unitika Ltd.
Charpy Impact Unnotched 8.20 J/cm²

@Temperature -30.0 °C
39.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled
injection molding grade20 % Glass fiber reinforcedgood heat resistancelow coefficent of linear thermal expansionApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. W..
Charpy Impact Unnotched 8.20 J/cm²
39.0 ft-lb/in²
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Charpy Impact Unnotched 8.20 J/cm²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 8.20 J/cm²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 8.20 J/cm²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r..