Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Charpy Impact Unnotched 9.20 J/cm²

@Temperature 23.0 °C
43.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1/XCF/40 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned
Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific)
PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ..
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179-1
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned
Information provided by Unitika Ltd.
Charpy Impact Unnotched 9.20 J/cm²

@Temperature 23.0 °C
43.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 9.20 J/cm²

@Temperature 23.0 °C
43.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)
Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding.