Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProduct Applications: TECHNYL B 218L V30 noir 44N is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is commonly used for automotive applications which require a good surface appearance and a good UV resistance, such as: external mirror housings and door handles. This product is available in black color.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527 Type 1A
Elongation at Break 8.0 %
8.0 %
ISO 527 Type 1A
Tensile Modulus 5.90 GPa
856 ksi
ISO 527 Type 1A
Flexural Strength 140 MPa
20300 psi
ISO 178
Flexural Modulus 4.70 GPa
682 ksi
ISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²
9.04 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
IEC 60243
Comparative Tracking Index 325 V
325 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: