Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Charpy Impact Unnotched | 11.0 J/cm² - NB | 52.4 ft-lb/in² - NB | Average value: 14.6 J/cm² Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
Polimeri Europa SINKRAL A22V ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 Very high flow grade for fast cycle injection moulding. Particularly recommended for the domestic .. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
Polimeri Europa SINKRAL B232/E ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EGN,105-04-09-25 Extrusion and thermoforming grade with good thermal resistance, high stiffness and a very low vol.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL G320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 448 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® H604 Standard impact strength.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® M305 Grade for smart cards, good dimensional accuracy, excellent dynamic loading capacity.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179 |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179/1eU |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179 |
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer Injection Molding, High rigidity |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
BASF Novolen® 1040 N Polypropylene Nucleated grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Conditioned) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade Grade for injection molded parts. Also available as a special grade for fibers (short spinning) and cast film.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL F233 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-15-16-25 Medium heat injection moulding grade having high flow and good thermal stability during processing.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL PD F332 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MGN,105-15-16-20 General purpose injection grade which combines excellent thermal stability during processing with.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | |
Polimeri Europa SINKRAL H220 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 General purpose, high flow injection moulding grade having good rigidity coupled with an excellent.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.4 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL L320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an .. |
|||
Charpy Impact Unnotched | 11.0 J/cm² | 52.4 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |